Nickel-Based Superalloys

Table of Contents

Overview

Nickel-based superalloys are the backbone of modern high-performance engineering applications, especially in industries that demand extreme durability and resistance to high temperatures. These superalloys are a marvel of material science, exhibiting exceptional strength, oxidation resistance, and creep resistance. They are predominantly used in aerospace, power generation, and chemical processing industries, where components face severe operational environments.

Key Highlights of Nickel-Based Superalloys:

  • Superior high-temperature performance
  • Exceptional mechanical strength
  • High resistance to thermal creep deformation
  • Good surface stability
  • Corrosion and oxidation resistance

Understanding these alloys in depth requires exploring their composition, properties, applications, and more. So, let’s dive right in and uncover the intricate details of these fascinating materials.

titanium alloy Ti64

Composition and Properties of Nickel-Based Superalloys

Nickel-based superalloys are primarily composed of nickel, chromium, cobalt, molybdenum, and aluminum, with minor additions of other elements like titanium, tungsten, and rhenium. The precise composition can vary significantly depending on the specific alloy and its intended application.

Table: Types, Composition, Properties, and Characteristics of Nickel-Based Superalloys

Alloy NameCompositionKey PropertiesCharacteristics
Inconel 718Ni-52%, Cr-19%, Fe-18%, Nb-5%, Mo-3%, Ti-1%, Al-0.5%Excellent tensile strength and rupture resistance at high tempsPrecipitation hardenable, good weldability
Hastelloy XNi-47%, Cr-22%, Fe-18%, Mo-9%, Co-1.5%, W-0.6%Outstanding oxidation resistance, good formabilityResistant to oxidizing and reducing environments
WaspaloyNi-58%, Cr-19%, Co-13%, Mo-4.3%, Ti-3%, Al-1.4%High strength and oxidation resistance at temperatures up to 870°CUsed in gas turbines and high-speed airframes
Rene 41Ni-53%, Cr-19%, Co-11%, Mo-10%, Ti-3%, Al-1.5%Superior high-temperature strength, oxidation resistanceUsed in turbine blades, die-casting applications
Nimonic 80ANi-76%, Cr-19.5%, Ti-2.5%, Al-1.4%, Fe-0.5%Good corrosion and oxidation resistance, high creep resistanceUsed in gas turbine components, nuclear reactors
Alloy 625Ni-61%, Cr-21.5%, Mo-9%, Nb-3.6%, Fe-2.5%, C-0.1%Excellent fatigue and thermal-fatigue propertiesUsed in aerospace, marine, and chemical processing
Haynes 282Ni-57%, Cr-19.5%, Co-10.5%, Mo-8.5%, Ti-2.1%, Al-1.5%, Fe-1.5%, Mn-0.06%, Si-0.15%, C-0.06%High creep strength, good thermal stabilitySuitable for gas turbines and other high-temp applications
Incoloy 800Ni-32.5%, Fe-46%, Cr-21%, C-0.05%, Mn-1.5%, Si-1%, Al-0.4%, Ti-0.4%Excellent resistance to oxidation, carburizationUsed in heat exchangers, furnace parts
Mar-M247Ni-60%, Cr-10%, Co-10%, W-10%, Al-5.5%, Ti-1%, Ta-3%, Hf-1.5%, C-0.15%, B-0.015%, Zr-0.05%Excellent creep resistance and high-temperature strengthUsed in turbine blades, aerospace applications
Udimet 720Ni-58%, Cr-19%, Co-15%, Mo-3%, Ti-5%, Al-2.5%, Fe-0.5%, C-0.03%High tensile and rupture strength, excellent oxidation resistanceUsed in gas turbine engines, high-stress environments

Applications of Nickel-Based Superalloys

Nickel-based superalloys find applications in several demanding environments due to their outstanding properties. Here, we’ll explore some key applications where these superalloys are indispensable.

Table: Applications and Uses of Nickel-Based Superalloys

IndustryApplicationDetails
AerospaceTurbine BladesHigh strength and oxidation resistance at elevated temperatures ensure efficiency and durability
Power GenerationGas Turbine ComponentsWithstand high thermal stresses and corrosive environments for long operational lifetimes
Chemical ProcessingHeat Exchangers and ReactorsExcellent resistance to corrosive chemicals and high temperatures, ensuring safe and efficient processes
MarineSubmarine PartsCorrosion resistance in seawater and strength to withstand high pressures
AutomotiveTurbocharger WheelsEnhanced performance at high temperatures and rotational speeds
Oil and GasDrilling EquipmentHigh wear resistance and strength to endure harsh drilling conditions
NuclearReactor Core ComponentsExcellent radiation resistance and thermal stability
MedicalProsthetics and ImplantsBiocompatibility and corrosion resistance for long-term reliability
ElectronicsHigh-Temperature ElectronicsStability and performance in extreme thermal environments
DefenseJet Engines and Missile ComponentsReliability and performance under extreme operational conditions

Specifications, Sizes, Grades, and Standards

The specifications, sizes, grades, and standards for nickel-based superalloys vary depending on their application and the industry requirements. Here’s a comprehensive table summarizing these details.

Table: Specifications, Sizes, Grades, and Standards for Nickel-Based Superalloys

Alloy NameSpecificationSizesGradesStandards
Inconel 718AMS 5662, ASTM B637Bars: 0.5-12 inches diameterUNS N07718AMS, ASTM, ISO
Hastelloy XAMS 5536, ASTM B435Sheets: 0.015-0.187 inches thickUNS N06002AMS, ASTM
WaspaloyAMS 5706, ASTM B637Bars: 0.5-6 inches diameterUNS N07001AMS, ASTM
Rene 41AMS 5545, AMS 5712Sheets: 0.02-0.187 inches thickUNS N07041AMS, ASTM
Nimonic 80AAMS 5828, ASTM B637Bars: 0.25-8 inches diameterUNS N07080AMS, ASTM, ISO
Alloy 625AMS 5666, ASTM B446Bars: 0.5-12 inches diameterUNS N06625AMS, ASTM, ASME
Haynes 282AMS 5914, ASTM B572Bars: 0.5-6 inches diameterUNS N07208AMS, ASTM, ASME
Incoloy 800ASTM B408, AMS 5766Bars: 0.25-10 inches diameterUNS N08800ASTM, ASME, ISO
Mar-M247Proprietary SpecsCastings: custom sizesProprietary
Udimet 720AMS 5664, ASTM B637Bars: 0.5-8 inches diameterUNS N07720AMS, ASTM, ASME

Suppliers and Pricing Details of Nickel-Based Superalloys

Finding reliable suppliers and understanding pricing details are crucial for industries relying on nickel-based superalloys. Here’s a table outlining some leading suppliers and pricing information.

Table: Suppliers and Pricing Details of Nickel-Based Superalloys

Supplier NameAlloys AvailablePricing Range (per kg)LocationContact Information
ATI MetalsInconel 718, Hastelloy X$50 – $100USAwww.atimetals.com, +1 800-289-8443
Haynes InternationalHaynes 282, Hastelloy X$70 – $120USAwww.haynesintl.com, +1 765-456-6000
Special MetalsNimonic 80A, Incoloy 800$60 – $110UK, USAwww.specialmetals.com, +1 304-526-5100
Carpenter TechnologyWaspaloy, Alloy 625$80 – $130USA, Europewww.cartech.com, +1 610-208-2000
VSMPO-AVISMARene 41, Mar-M247$90 – $150Russiawww.vsmpo.ru, +7 343 45 55 204
VDM MetalsAlloy 625, Inconel 718$70 – $120Germanywww.vdm-metals.com, +49 2392 55-0
Allegheny TechnologiesInconel 718, Alloy 625$50 – $110USA www.atimetals.com, +1 800-289-8443
Arconic Udimet 720, Rene 41$100 – $160USA, Globalwww.arconic.com, +1 412-315-2900
Erasteel Nimonic 80A, Waspaloy$80 – $140France www.erasteel.com, +33 1 53 32 30 00
Precision Castparts CorpMar-M247, Waspaloy$90 – $150USA, Globalwww.precast.com, +1 503-946-4800

Advantages of Nickel-Based Superalloys

Nickel-based superalloys boast several advantages that make them the material of choice for high-stress, high-temperature applications. Let’s delve into some of the key benefits.

Table: Advantages of Nickel-Based Superalloys

AdvantageDescription
High Temperature ResistanceMaintain strength and stability at temperatures exceeding 1000°C
Corrosion ResistanceResistant to oxidation, sulfidation, and other forms of high-temperature corrosion
Mechanical StrengthExceptional tensile and rupture strength, crucial for high-stress environments
Creep ResistanceMinimize deformation under prolonged exposure to high stresses and temperatures
Fatigue ResistanceHigh resistance to fatigue, making them ideal for cyclic loading conditions
VersatilitySuitable for a wide range of industries including aerospace, power generation, and chemical processing
DurabilityLong operational lifetimes even in extreme environments
Thermal StabilityStable mechanical properties across a wide temperature range
MachinabilityCan be machined to precise specifications, essential for complex component design
CustomizabilityAlloy compositions can be tailored to specific application requirements

Disadvantages of Nickel-Based Superalloys

Despite their numerous advantages, nickel-based superalloys have certain limitations. Here’s a look at some of the potential drawbacks.

Table: Disadvantages of Nickel-Based Superalloys

DisadvantageDescription
High CostExpensive due to the cost of raw materials and complex manufacturing processes
Machining ChallengesDifficult to machine compared to other materials, requiring specialized tools and techniques
DensityRelatively high density, which can be a drawback in weight-sensitive applications
AvailabilityLimited availability of certain alloys and grades, potentially leading to longer lead times
Recycling ComplexityRecycling these superalloys is challenging due to their complex compositions
Fabrication DifficultyRequires advanced fabrication techniques, which can be time-consuming and costly
Thermal ConductivityLower thermal conductivity compared to some other high-temperature materials
Environmental ImpactExtraction and processing of raw materials can have significant environmental impacts
Allergic ReactionsPotential for nickel allergies in some individuals
Limited SuppliersFewer suppliers with the capability to produce high-quality superalloys, affecting market competition

Comparison of Nickel-Based Superalloys

Comparing various nickel-based superalloys helps in selecting the right material for specific applications. Here’s a detailed comparison based on key parameters.

Table: Comparison of Nickel-Based Superalloys

AlloyStrengthTemperature ResistanceCorrosion ResistanceMachinabilityCost
Inconel 718HighUp to 700°CExcellentGoodModerate
Hastelloy XModerateUp to 1200°COutstandingFairHigh
WaspaloyVery HighUp to 870°CGoodFairHigh
Rene 41Very HighUp to 1000°CExcellentDifficultHigh
Nimonic 80AHighUp to 815°CGoodGoodModerate
Alloy 625HighUp to 982°CExcellentGoodHigh
Haynes 282Very HighUp to 980°CGoodFairHigh
Incoloy 800ModerateUp to 700°CExcellentGoodModerate
Mar-M247Very HighUp to 1150°CGoodDifficultVery High
Udimet 720Very HighUp to 950°CExcellentFairHigh
nickel-based superalloys

FAQs

Table: Frequently Asked Questions about Nickel-Based Superalloys

QuestionAnswer
What are nickel-based superalloys?High-performance alloys primarily composed of nickel, designed for extreme environments.
What industries use nickel-based superalloys?Aerospace, power generation, chemical processing, marine, automotive, and more.
Why are nickel-based superalloys expensive?Due to the cost of raw materials and the complex manufacturing processes involved.
Can nickel-based superalloys be recycled?Yes, but recycling is complex due to their intricate compositions.
What is the temperature limit for nickel-based superalloys?They can withstand temperatures up to 1200°C depending on the alloy.
Are there any health concerns with nickel-based superalloys?Potential nickel allergies in some individuals.
How are nickel-based superalloys manufactured?Through processes like casting, forging, and powder metallurgy.
What makes nickel-based superalloys corrosion resistant?High chromium content and other alloying elements provide excellent corrosion resistance.
Can these superalloys be welded?Yes, but welding requires specific techniques and post-weld treatments.
How do nickel-based superalloys compare to other superalloys?They generally offer superior high-temperature performance and corrosion resistance.

Conclusion

Nickel-based superalloys are essential materials that drive performance in some of the most challenging engineering environments. Their remarkable properties make them indispensable in industries where failure is not an option. By understanding their composition, properties, applications, and the trade-offs involved, engineers and material scientists can make informed decisions that push the boundaries of technology and innovation.

So, the next time you see a jet engine or a gas turbine, remember the unsung heroes – the nickel-based superalloys – working tirelessly behind the scenes to keep the world running smoothly.

know more 3D printing processes

Share On

Facebook
Twitter
LinkedIn
WhatsApp
Email

Xmetto Technology Co., LTD is a leading provider of additive manufacturing solutions headquartered in Qingdao, China. Our company specializes in 3D printing equipment and high-performance metal powders for industrial applications.

Inquiry to get best price and customized Solution for your business!

Related Articles